Solidification of sand by Pb(II)-tolerant bacteria for ...
Sand biocemented by KBZ 1-3 and KBZ 2-5 had maximum unconfined compressive strength values of 3.2 MPa and 5.5 MPa, respectively. Additionally, biocemented sand exhibited reduced water permeability values of 9.6 × 10-8 m/s and 8.9 × 10-8 m/s for O. profundus KBZ 1-3 and KBZ 2-5, respectively, which could potentially limit the entrance of water ...